{"_buckets": {"deposit": "3f3d9176-1d56-4c27-ad67-44abe9492441"}, "_deposit": {"created_by": 3, "id": "4000", "owners": [3], "pid": {"revision_id": 0, "type": "depid", "value": "4000"}, "status": "published"}, "_oai": {"id": "oai:ynu.repo.nii.ac.jp:00004000", "sets": ["496"]}, "author_link": ["17903", "17901", "480"], "item_2_biblio_info_8": {"attribute_name": "書誌情報", "attribute_value_mlt": [{"bibliographicIssueDates": {"bibliographicIssueDate": "2009", "bibliographicIssueDateType": "Issued"}, "bibliographicIssueNumber": "1", "bibliographicPageEnd": "131", "bibliographicPageStart": "124", "bibliographicVolumeNumber": "49", "bibliographic_titles": [{"bibliographic_title": "ISIJ international"}]}]}, "item_2_description_17": {"attribute_name": "フォーマット", "attribute_value_mlt": [{"subitem_description": "application/pdf", "subitem_description_type": "Other"}]}, "item_2_description_5": {"attribute_name": "抄録", "attribute_value_mlt": [{"subitem_description": "Fatigue crack growth modeling was performed for Ti-6Al-4V forged materials failed by subsurface crack generation at cryogenic temperatures. The modeling that was based on linear fracture mechanics under the Mode I condition provided a good estimate of the stress intensity range of subsurface or surface and fatigue crack growth, enabling the estimation of the crack propagation life. The fatigue crack growth rate calculated using the Paris rule, da/dN=C(ΔK_1)^m, almost corresponded to the one obtained from the analysis of the striation on the fracture surface. The calculated crack propagation life was less than a tenth of the number of cycles to failure over 10^6. As a result, the subsurface crack initiation (Stage I crack generation) process consumed a large number of cycles to failure-as many as that at a lower stress level.", "subitem_description_type": "Abstract"}]}, "item_2_full_name_2": {"attribute_name": "著者(ヨミ)", "attribute_value_mlt": [{"nameIdentifiers": [{"nameIdentifier": "17903", "nameIdentifierScheme": "WEKO"}], "names": [{"name": "ハマダ, マキコ"}]}, {"nameIdentifiers": [{"nameIdentifier": "480", "nameIdentifierScheme": "WEKO"}, {"nameIdentifier": "20343171", "nameIdentifierScheme": "e-Rad", "nameIdentifierURI": "https://kaken.nii.ac.jp/ja/search/?qm=20343171"}], "names": [{"name": "ウメザワ, オサム"}]}]}, "item_2_publisher_35": {"attribute_name": "出版者", "attribute_value_mlt": [{"subitem_publisher": "日本鉄鋼協会"}]}, "item_2_relation_13": {"attribute_name": "DOI", "attribute_value_mlt": [{"subitem_relation_type": "isIdenticalTo", "subitem_relation_type_id": {"subitem_relation_type_id_text": "10.2355/isijinternational.49.124", "subitem_relation_type_select": "DOI"}}]}, "item_2_rights_14": {"attribute_name": "権利", "attribute_value_mlt": [{"subitem_rights": "?日本鉄鋼協会"}]}, "item_2_rights_15": {"attribute_name": "権利URI", "attribute_value_mlt": [{"subitem_rights": "www.isij.or.jp | www.isij.or.jp"}]}, "item_2_source_id_11": {"attribute_name": "書誌レコードID", "attribute_value_mlt": [{"subitem_source_identifier": "AA10680712", "subitem_source_identifier_type": "NCID"}]}, "item_2_source_id_9": {"attribute_name": "ISSN", "attribute_value_mlt": [{"subitem_source_identifier": "09151559", "subitem_source_identifier_type": "ISSN"}]}, "item_2_text_4": {"attribute_name": "著者所属", "attribute_value_mlt": [{"subitem_text_value": "Department of Materials Science and Engineering, Graduate School of Engineering, Yokohama National University"}, {"subitem_text_value": "Department of Materials Science and Engineering, Graduate School of Engineering, Yokohama National University"}]}, "item_2_version_type_18": {"attribute_name": "著者版フラグ", "attribute_value_mlt": [{"subitem_version_resource": "http://purl.org/coar/version/c_970fb48d4fbd8a85", "subitem_version_type": "VoR"}]}, "item_creator": {"attribute_name": "著者", "attribute_type": "creator", "attribute_value_mlt": [{"creatorNames": [{"creatorName": "Hamada, Makiko"}], "nameIdentifiers": [{"nameIdentifier": "17901", "nameIdentifierScheme": "WEKO"}]}, {"creatorNames": [{"creatorName": "Umezawa, Osamu"}], "nameIdentifiers": [{"nameIdentifier": "480", "nameIdentifierScheme": "WEKO"}, {"nameIdentifier": "20343171", "nameIdentifierScheme": "e-Rad", "nameIdentifierURI": "https://kaken.nii.ac.jp/ja/search/?qm=20343171"}]}]}, "item_files": {"attribute_name": "ファイル情報", "attribute_type": "file", "attribute_value_mlt": [{"accessrole": "open_date", "date": [{"dateType": "Available", "dateValue": "2016-09-16"}], "displaytype": "detail", "download_preview_message": "", "file_order": 0, "filename": "A-55 ISIJ49_1.pdf", "filesize": [{"value": "497.7 kB"}], "format": "application/pdf", "future_date_message": "", "is_thumbnail": false, "licensetype": "license_free", "mimetype": "application/pdf", "size": 497700.0, "url": {"label": "A-55 ISIJ49_1.pdf", "url": "https://ynu.repo.nii.ac.jp/record/4000/files/A-55 ISIJ49_1.pdf"}, "version_id": "27e12b6c-3a23-47ff-8ce4-84a8ffad4e62"}]}, "item_keyword": {"attribute_name": "キーワード", "attribute_value_mlt": [{"subitem_subject": "fractography", "subitem_subject_scheme": "Other"}, {"subitem_subject": "subsurface crack initiation", "subitem_subject_scheme": "Other"}, {"subitem_subject": "fatigue crack growth", "subitem_subject_scheme": "Other"}, {"subitem_subject": "titanium alloy", "subitem_subject_scheme": "Other"}]}, "item_language": {"attribute_name": "言語", "attribute_value_mlt": [{"subitem_language": "eng"}]}, "item_resource_type": {"attribute_name": "資源タイプ", "attribute_value_mlt": [{"resourcetype": "journal article", "resourceuri": "http://purl.org/coar/resource_type/c_6501"}]}, "item_title": "Evaluation of subsurface fatigue crack life in forged Ti-6Al-4V alloys at cryogenic temperatures", "item_titles": {"attribute_name": "タイトル", "attribute_value_mlt": [{"subitem_title": "Evaluation of subsurface fatigue crack life in forged Ti-6Al-4V alloys at cryogenic temperatures"}]}, "item_type_id": "2", "owner": "3", "path": ["496"], "permalink_uri": "http://hdl.handle.net/10131/7926", "pubdate": {"attribute_name": "公開日", "attribute_value": "2012-03-23"}, "publish_date": "2012-03-23", "publish_status": "0", "recid": "4000", "relation": {}, "relation_version_is_last": true, "title": ["Evaluation of subsurface fatigue crack life in forged Ti-6Al-4V alloys at cryogenic temperatures"], "weko_shared_id": 3}
Evaluation of subsurface fatigue crack life in forged Ti-6Al-4V alloys at cryogenic temperatures
http://hdl.handle.net/10131/7926
http://hdl.handle.net/10131/792655307bad-2d76-4cfa-9db2-26e627f36f0e
名前 / ファイル | ライセンス | アクション |
---|---|---|
A-55 ISIJ49_1.pdf (497.7 kB)
|
|
Item type | 学術雑誌論文 / Journal Article(1) | |||||
---|---|---|---|---|---|---|
公開日 | 2012-03-23 | |||||
タイトル | ||||||
タイトル | Evaluation of subsurface fatigue crack life in forged Ti-6Al-4V alloys at cryogenic temperatures | |||||
言語 | ||||||
言語 | eng | |||||
キーワード | ||||||
主題 | fractography, subsurface crack initiation, fatigue crack growth, titanium alloy | |||||
資源タイプ | ||||||
資源タイプ識別子 | http://purl.org/coar/resource_type/c_6501 | |||||
資源タイプ | journal article | |||||
著者 |
Hamada, Makiko
× Hamada, Makiko× Umezawa, Osamu |
|||||
著者(ヨミ) | ||||||
識別子Scheme | WEKO | |||||
識別子 | 17903 | |||||
姓名 | ハマダ, マキコ | |||||
著者(ヨミ) | ||||||
識別子Scheme | WEKO | |||||
識別子 | 480 | |||||
識別子Scheme | e-Rad | |||||
識別子URI | https://kaken.nii.ac.jp/ja/search/?qm=20343171 | |||||
識別子 | 20343171 | |||||
姓名 | ウメザワ, オサム | |||||
著者所属 | ||||||
Department of Materials Science and Engineering, Graduate School of Engineering, Yokohama National University | ||||||
著者所属 | ||||||
Department of Materials Science and Engineering, Graduate School of Engineering, Yokohama National University | ||||||
抄録 | ||||||
内容記述タイプ | Abstract | |||||
内容記述 | Fatigue crack growth modeling was performed for Ti-6Al-4V forged materials failed by subsurface crack generation at cryogenic temperatures. The modeling that was based on linear fracture mechanics under the Mode I condition provided a good estimate of the stress intensity range of subsurface or surface and fatigue crack growth, enabling the estimation of the crack propagation life. The fatigue crack growth rate calculated using the Paris rule, da/dN=C(ΔK_1)^m, almost corresponded to the one obtained from the analysis of the striation on the fracture surface. The calculated crack propagation life was less than a tenth of the number of cycles to failure over 10^6. As a result, the subsurface crack initiation (Stage I crack generation) process consumed a large number of cycles to failure-as many as that at a lower stress level. | |||||
書誌情報 |
ISIJ international 巻 49, 号 1, p. 124-131, 発行日 2009 |
|||||
ISSN | ||||||
収録物識別子タイプ | ISSN | |||||
収録物識別子 | 09151559 | |||||
書誌レコードID | ||||||
収録物識別子タイプ | NCID | |||||
収録物識別子 | AA10680712 | |||||
DOI | ||||||
関連タイプ | isIdenticalTo | |||||
識別子タイプ | DOI | |||||
関連識別子 | 10.2355/isijinternational.49.124 | |||||
権利 | ||||||
権利情報 | ?日本鉄鋼協会 | |||||
権利URI | ||||||
権利情報 | www.isij.or.jp | www.isij.or.jp | |||||
フォーマット | ||||||
内容記述タイプ | Other | |||||
内容記述 | application/pdf | |||||
著者版フラグ | ||||||
出版タイプ | VoR | |||||
出版タイプResource | http://purl.org/coar/version/c_970fb48d4fbd8a85 | |||||
出版者 | ||||||
出版者 | 日本鉄鋼協会 |